48,241 views
Note. In the settling tanks, after three days of settling, I collected another 2.97 grams. Detailed process of silver melange. Recycled plugs 6P-100, 6P-150V. Through silver sulfate, crystal clear silver chloride is obtained. The same sockets remained. I used available reagents, this is an electrolyte salt ammonium nitrate. Otherwise, the usual melange process, passivation of the base with concentrated sulfuric acid, and restoration of chloride through cementation on aluminum. ************************************************************************* The channel will have videos about what I do and how. I am not a professional, but an amateur - so you can see not how everything is wonderful and super, but real problems and ways to solve them, as well as proven working methods. There will be everything - both sad and happy. Each of you will find something close to your heart. Subscribe, click the bell, thumbs up and write a comment - it's free, and then everything will be fine ))) You can write to me by email and it is advisable to let me know in the comments - [email protected], or better yet, Vkontakte https://vk.com/id587946420 And you can even provide financial assistance for the development of the channel, if you have the desire and opportunity. https://yoomoney.ru/to/410016681700033 If you are going to violate my rights, let me know. All the methods I show are in open sources and are publicly available. All videos are staged, posted for informational and entertainment purposes, are not advertising or a call to action. The author is not responsible for any consequences caused by the material of this video.