162,681 views
The video shows the process of processing contacts of processors in the amount of ~ 67 grams. After removing foreign metals such as copper and nickel, the resulting gold plating was dissolved in a mixture of hydrochloric acid and nitric (aqua regia) and then restoration was done - with hydrazine hydrochloride to elemental gold. Mail for communication: [email protected]